Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cornflower-blue magnetite (Fe3O4).
  
Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cornflower-blue magnetite (Fe3O4).
+
[[Category:Glossary]]

Version vom 18. Februar 2010, 01:16 Uhr

Blued steel

Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cornflower-blue magnetite (Fe3O4).