(Die Seite wurde neu angelegt: '''Blued steel''' Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cor...) |
|||
| (5 dazwischenliegende Versionen von 2 Benutzern werden nicht angezeigt) | |||
| Zeile 1: | Zeile 1: | ||
'''Blued steel''' | '''Blued steel''' | ||
| + | |||
| + | Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cornflower-blue magnetite (Fe3O4). | ||
| + | |||
| + | [[Category:Glossary]] | ||
| − | + | [[de:Gebläuter Stahl]] | |
| + | [[en:Blued steel]] | ||
| + | [[es:Acero de Blued]] | ||
| + | [[fr:Acier oxydé]] | ||
| + | [[pt:Aço de Blued]] | ||
| + | [[ru:Воронёная сталь]] | ||
Aktuelle Version vom 13. Juni 2015, 00:41 Uhr
Blued steel
Steel parts are slowly and cautiously heated (annealed) to about 300°C. This process coats the metal with an extremely thin, shimmering film of cornflower-blue magnetite (Fe3O4).